Hollow-sounding tiles and loose edges are almost always an adhesive mismatch, not bad workmanship. The grade is chosen by two things.
Cement and sand still goes down on plenty of floors, and on small ceramic tiles over a good screed it works. It stops working the moment the tile gets large, dense or vertical — which describes most tiles sold today.
Why vitrified tiles need adhesive
Traditional mortar bonds by absorption: water moves from the mortar into a porous tile and the cement crystallises in the pores. Vitrified tiles are almost non-porous. There is nothing for the mortar to grip, so the bond relies on friction alone — which is why those tiles start sounding hollow and lifting at the corners a year later.
Tile adhesive bonds chemically instead, with polymers that grip a smooth back.
The grades, simply
- Type 1 — internal floors and walls, ceramic tiles, normal conditions. The everyday grade.
- Type 2 — higher bond strength. Vitrified tiles, wet areas, external walls at low level.
- Type 3 — high strength and more flexible. Large-format tiles, tile-on-tile, façades, swimming pools, glass mosaic.
- Type 4 — heavy-duty and highly flexible. Industrial floors, heated floors, substrates that move.
- Epoxy — chemical resistance and zero water absorption. Kitchens, labs, dairies, acid-exposed areas.
Choose by the pair, not the tile alone
The grade follows the combination of tile and substrate. The same vitrified tile needs one grade over a fresh screed and a higher one over existing tiles, because the substrate offers less grip. Tile-on-tile always moves up a grade.
Grout is not an afterthought
Cement grout is fine for dry internal areas. For bathrooms, kitchen counters and anywhere that gets cleaned with chemicals, epoxy grout is worth the extra — it does not absorb water, does not stain, and does not grow the black line along the shower floor.
Common mistakes
- Too little coverage. Notched trowel on the substrate, and on the back of the tile for large formats. Aim for near-full contact — voids are where cracks start.
- Mixing too much at once. Adhesive has a working life. Mix what the team will lay in that window.
- Adding extra water to re-soften. Once it has started setting, it is finished. Re-tempering destroys the bond.
- Skipping levelling. Adhesive is not a levelling compound. An uneven floor needs a levelling screed first.
Rough quantities
For normal tiles on a flat surface, plan on roughly 4–5 kg of adhesive per square metre. Large-format tiles or an uneven substrate push that higher. Bring your area and tile size to the counter and we will work it out properly.